Customization: | Available |
---|---|
Bonding Function: | Structural Adhesive |
Morphology: | Liquid |
Still deciding? Get samples of US$ 5/kg
Request Sample
|
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
No. |
Items |
Technical data |
|
1 |
Appearance |
Part A |
colorless and transparent liquid |
Part B |
colorless and transparent liquid |
||
2 |
Viscosity (mPa·s) |
Part A |
600-1000 |
Part B |
30-60 |
||
3 |
Mix ratio(A∶B) |
4 :1 |
|
4 |
Pot life(25ºC,min) |
10-15 |
|
5 |
Initial curing time(25ºC,h) |
2-3 |
|
6 |
Shear Strength(RT48h,MPa) |
≥7.0 |
Curing Time
Temperature(ºC) |
Pot life (min) |
Initial curing time(h) |
5-10 |
20-30 |
6-8 |
10-20 |
15-20 |
4-6 |
20-30 |
10-15 |
3-4 |
30-40 |
5-10 |
2-3 |
[Performance Characteristics]
The product is in low viscosity and high penetration. It has strong adhesion and strength after cured.It is abrasion, water, oil, chemical and aging resistant. The glue layer is colorless and transparent and anti yellowing.
[Instructions]
1. Slabs treatment
Slabs should be totally dry.
Remove the mud, oil or other purity on the slab surface.
2. Prepare the glue and mix
Mix the glue by A:B=4:1(by weight) completely
Please use up the glue within the pot life. The glue will be fever and is prohibited to use when beyond the pot life. The more of the glue mixed, and the higher of the temperature, the shorter the pot life. If mixed too much glue, please divide quickly to use.
Do not mix the cap of A and B. Please seal the caps anytime in case the moisture and dash from the air.
The plated with big open mouth container is recommend for glue mixing to extend the pot life of glue
3. Spreading the glue
Spread the glue evenly on the surface of slab with scrape back and forth. The recommend using weight is 80-150g/.
For the cracks on slabs, spread glue back and forth to make the glue penetrate completely.
For the big defects on the slab, such as the soil, please remove first, then mix the glue and stone powder to fix it. Polish after cured, then spread the glue.
Please do not use the non epoxy and other slab surface treatment agent, or it will be not suitable for the epoxy glue spreading.
4. Glue solidify
The glue will be initially cured in 2-3 house under room temperature(25ºC)It can be proceed to next procedure after 24 hours;
If possible, heat up the stone with adhesive to 50-60 ºC and polish it after 2-3 hours.
Before the adhesive cured, the stone should be placed horizontally and not stacked; after cured, the lubricants such as talcum powder can be applied on the stone surface, to avoid stone adhesion when they are stacked.
5. Clean up
Use the specialized cleaner to clean the apparatus before the glue cured.