Fissures/Crack Filling Epoxy Glue for Marble & Granite

Product Details
Customization: Available
Bonding Function: Liquid Sealing Leak
Morphology: Clear Liquid
Still deciding? Get samples of US$ 1/Piece
Request Sample

360° Virtual Tour

Diamond Member Since 2014

Suppliers with verified business licenses

Audited Supplier

Audited by an independent third-party inspection agency

to see all verified strength labels (23)
  • Fissures/Crack Filling Epoxy Glue for Marble & Granite
  • Fissures/Crack Filling Epoxy Glue for Marble & Granite
  • Fissures/Crack Filling Epoxy Glue for Marble & Granite
  • Fissures/Crack Filling Epoxy Glue for Marble & Granite
  • Fissures/Crack Filling Epoxy Glue for Marble & Granite
  • Fissures/Crack Filling Epoxy Glue for Marble & Granite
Find Similar Products

Basic Info.

Model NO.
sk1150
Material
Epoxy
Classification
Stone Epoxy
Main Agent Composition
Epoxy, Hardner
Characteristic
Waterproof
Promoter Composition
Curing Agent
Composition
Inorganic Material
Color
Clear
Transport Package
Plastic Drum
Specification
500G, 1KG, 5KG, 25KG, 200KG, 1000kg
Trademark
MAGPOW
Origin
Changsha, Hunan
HS Code
3506100090
Production Capacity
1000tons/Year

Product Description

clear Fissures/Crack Filling Epoxy Glue for marble & granite
 
Item No.: 1150
 
Mix ratio by weight: A:B=4:1
 
Application: The product is used for repairing irregular cracks like micro-cracks, (sand holes, chicken patterns, ant roads) and uneven patches on the surface of various stones.

[Protection Measures]

For different workers, the glue may irritate the skin, but the product meet national standard GB18583-2008, it is environmental friendly and no harm to human body.

When using this glue, please take the protections as below:

Use the glue in the ventilate environment

Wear the protection cloths, gloves and mask

In case the glue contact skin directly, if any, clean with the soap water

Before mix the glue, open the cap of Part B first, wait for the volatility of the free low molecular materials

If any irritation to the skin, better to change to other jobs.
 

[Cautions]

1.Some facts will affect the performance of the glue as below:

The stone is not dry enough or the air humidity is too high, the stone absorbed the moisture from air

Part A and B was not mixed exactly base on the stipulated ratio

Glue mix uneven or not completely 

Mixed the apparatus of A and B, the glue is cured in advance

The mixed glue was not used up within the pot life

2.In winter and low temperature, the product may form crystal or caking. Just heat up the glue     and make the crystal or caking dissolved, this will not affect the glue performance.

3.Clean and wipe the glue on cloth or skin before it cured with alcohol, then flush with soap  water. If in eyes, flush with plenty of water and seek for medical cure; if swallowed, do not emetic, drink plenty of egg white or milk, then seek for medical cure immediately. 
 

Technical data

No.

Project

Technical data

1

Appearance

A  component

Colorless transparent liquid

B  component

Colorless transparent liquid

2

Viscosity(mPa·s)

A  component

600-1000

B  component

10-30

3

Adjusting ratio(AB)

31

4

Applicable period(25ºC,min)

60-90

5

Initial curing time(25ºC,h)

3-4

6

Tensile shear strength(RT48h,MPa)

7.0


PS: The time above is based on the mixed glue 600g
 

[Stock and Package]

1.Sealed and stock in cool, dry and ventilate place, stock temperature under 5-40ºC. Shelf life one year from the production date, it can be still used based on passing the test when beyond the shelf life. 

2.This product is corrosive goods, keep far away from the heat, fire, sunshine and rain during delivery and stock. In the process of transportation, operate gently, it is prohibited to roll, impact, stress, inversion, and offset

3.Packing size: 100Kg/set, in plastic drum packing. 1000kg/set, Part A in Iron drum packing and B in plastic drum packing. 

 

[Important Notes]

1.For materials to be bond are different, this may affect the glue performance. Please have a try before plenty use.

2.We solemn promise: we produce the products according to our enterprise standard strictly, we will responsible for the product quality, but not responsible for the operation process.

3.To provide the certified products to our customers, we operate strictly according to Quality systemISO9001 and Environmental management system ISO14001. Our technology suggestions in oral, written and experiment is from our honestly, which can not be our guarantee. Please read the instructions carefully before use, also arrange testing to ensure the glue is suitable for your process and applications.

4.We can not control the goods stock & delivery, operate condition and process, we will not responsible for the quality and related lost from the incorrect operations.

5.Any employees from our company can not revise or disregard the terms above.

 

[Executive Standard]

Enterprise standard: Q/BVNR006-2018
Fissures/Crack Filling Epoxy Glue for Marble & GraniteFissures/Crack Filling Epoxy Glue for Marble & Granite

 

Fissures/Crack Filling Epoxy Glue for Marble & GraniteFissures/Crack Filling Epoxy Glue for Marble & GraniteFissures/Crack Filling Epoxy Glue for Marble & GraniteFissures/Crack Filling Epoxy Glue for Marble & GraniteFissures/Crack Filling Epoxy Glue for Marble & GraniteFissures/Crack Filling Epoxy Glue for Marble & GraniteFissures/Crack Filling Epoxy Glue for Marble & Granite

Send your message to this supplier

*From:
*To:
*Message:

Enter between 20 to 4,000 characters.

This is not what you are looking for? Post a Sourcing Request Now
Contact Supplier